Work sequence and interface-treatment requirements for section-enlargement strengthening of concrete members (GB 50550-2010 clauses 5.1.2, 5.2.1; CJJ/T 239-2016 clause 5.6.2; GB 50367-2013 clause 5.5.2; JGJ/T 112-2019 clause 6.4.2)
Sequence (GB 50550-2010 clause 5.1.2): clean and dress the original member -> fix the new bars (stirrup planting included) and tie to the original bars -> treat the interface -> fix formwork -> cast concrete -> cure and strike -> inspect quality. Interface (clause 5.2.1): after dressing the bond face to fresh aggregate, roughen by bush hammer (points about 3 mm deep at 600-800 per m2, or 4-5 mm deep on about 30 mm staggered centres), grinder or high-pressure water jet (grooves 3-4 mm deep at about 50 mm), or cut grooves (about 6 mm deep at 100-150 mm), then clear loose aggregate and dust and pressure-wash; the step is never omitted with or without structural interface adhesive. GB 50367-2013 clause 5.5.2: beyond roughening, brush structural interface adhesive, plant shear dowels or add shear keys to secure composite action of old and new concrete.
Applicable Codes
- GB 50550-2010 建筑结构加固工程施工质量验收规范
- GB 50367-2013 混凝土结构加固设计规范
- CJJ/T 239-2016 城市桥梁结构加固技术规程
- JGJ/T 112-2019 民用建筑修缮工程施工标准
Topic Positioning
The work sequence and interface (bond-face) treatment of section-enlargement strengthening for concrete members (beams, columns, slabs, walls, foundations), across building strengthening acceptance, civil-building repair and city-bridge strengthening codes.
Core Conclusions
1. Sequence (GB 50550-2010 clause 5.1.2) "Section-enlargement works of concrete members shall proceed: 1 clean and dress the original structure and members; 2 fix the new bars (stirrup planting included) and connect them to the original bars and stirrups; 3 treat the interface; 4 fix formwork; 5 cast concrete; 6 cure and strike; 7 inspect workmanship." Commentary: against ordinary cast-in-place work this adds dressing the original members, tying original to new bars, and treating the interface - decisive for composite action and most often missed by crews used to new-build; the method statement shall stress supervision and inspection of these three steps.
2. City bridges (CJJ/T 239-2016 clause 5.6.2) "Section enlargement of concrete members shall proceed: 1 clean and dress the original structure and members; 2 treat the interface; 3 plant bars or anchor bolts; 4 fabricate and fix the new bars; 5 fix formwork and cast concrete; 6 cure and strike; 7 inspect workmanship." Commentary: ordinary members thicken by formed casting; deck slabs may use the original member as the soffit without soffit formwork; arch-ring tops may use the original ring as the soffit.
3. Interface roughening (GB 50550-2010 clause 5.2.1) "After dressing the bond face of the original member to fresh aggregate, roughen by bush hammer, grinder or high-pressure water jet; where necessary, cut grooves." Requirements: 1 Bush hammering: a 1.5-2.5 kg pointed stone bush hammer pits the bond face to points about 3 mm deep at 600-800 per m2 evenly spread, or 4-5 mm deep on about 30 mm staggered (quincunx) centres. 2 Grinder or water-jet roughening: a roughing wheel of 340 W output or more, or a jet per annex C, cuts transverse grooves perpendicular to the member axis, 3-4 mm deep at about 50 mm. 3 Hand grooving: sharp chisels cut transverse grooves on sound concrete, perpendicular to the axis, about 6 mm deep at 100-150 mm. Where three- or four-face jackets encase beams or columns, chamfer the arrises while roughening. After working, brush off loose aggregate, grit, dust and slurry and pressure-wash clean; for shotcrete, alternate compressed air and water. Extent: all; method: look and touch; on dispute, re-measure mean depth with a depth gauge. Commentary: interface quality decides whether enlargement and original bond - the step is never omitted, with or without structural interface adhesive.
4. Interface measures (GB 50367-2013 clause 5.5.2) "Under section enlargement, the original concrete surface shall be treated, and the design documents shall state the method and quality required. Generally, beyond roughening, brush structural interface adhesive, plant shear dowels or add shear keys to secure composite action." Commentary: the designer fixes the treatment. For beams and columns, roughening plus interface adhesive generally satisfies safety; walls and slabs further take shear dowels, structurally arranged only. Where erecting bars and formwork outruns the adhesive's pot life, shear dowels alone may carry the interface shear - experience shows d6 L-shaped dowels planted 50 mm deep at 200-300 mm centres serve a roughened face.
5. Under-beam thickening / jackets (JGJ/T 112-2019 clause 6.4.2) "On thickening under beams or encasing them: 1 scabble the soffit and, every 500 mm, cut grooves 50-70 mm wide and 20-30 mm deep; 2 the new bars' bearing lengths and the bearing-section sizes follow the survey design; 3 prefer U-forms, striking the sides before final set and trimming the surplus concrete at both cheeks; 4 when casting through drilled holes in the slab above, holes at 500 mm centres, cutting no original bars; 5 the casting material preferably a free-flowing fine-gravel concrete or cement-based grout." Commentary: tests show the after-cast concrete tends to tear off under load - beyond scabbling, cut shear keys in the soffit.
Applicability Boundaries
- The three sequence clauses serve building strengthening acceptance, city-bridge strengthening and civil-building repair; the steps differ slightly (bridges list "bar planting or anchoring" as step 3; buildings fold it into fixing the new bars).
- The roughening parameters (bush points, groove depth, spacing) are GB 50550-2010's; the actual method and quality follow the design documents.
- Structural interface adhesive must match its pot life to bar and formwork time - past it, switch to the dowel scheme.
- Sequence and interface technique only; concrete grades and bar design follow GB 50367-2013.
Further Reading
- GB 50550-2010 Code for Acceptance of Strengthening Construction of Building Structures, clauses 5.1.2 and 5.2.1 with commentary and annex C (jet pressure)
- CJJ/T 239-2016 Technical Specification for Strengthening of City Bridges, clause 5.6.2
- GB 50367-2013 Code for Design of Strengthening Concrete Structures, clause 5.5.2 with commentary
- JGJ/T 112-2019 Standard for Repair Works of Civil Buildings, clause 6.4.2
Keywords
- 增大截面加固
- 施工程序
- 界面处理
- 原构件凿毛
- 结构界面胶
- 种植剪切销钉
- GB 50550-2010
- 新旧混凝土共同工作