Engineering Knowledge Cards.
Confidence HighUpdated 2026-10-13

Structural layering of permeable brick paving (sponge-city permeable paving), each layer's material / thickness / porosity requirements and construction control indices - also the build-up basis for pricing layer by layer

Permeable brick paving layers as surface of permeable bricks - levelling (bedding) layer - permeable base - permeable subbase (cushion) - subgrade, each layer differing in build-up and materials - the basis of design, construction and layer-by-layer quota itemisation. DB37/T 5060-2016 Article 5.2.7: surface preferably 60-80 mm, levelling layer 20-40 mm, cushion 100-300 mm, surface porosity at least 20% and permeable cushion at least 30%; DB11/T 685-2021 Article 7.2.12: the levelling layer's permeability coefficient shall be not less than the surface's; the permeable base may be graded crushed stone, porous cement-stabilised crushed stone or pervious concrete, thickness per the ground load intensity; DB3201/T 1150-2023 Article 5.3.1: subbase compaction at least 93%, dry-hard mortar bedding cement-sand 1:3, spreading thickness not under 20 mm, pervious concrete base joints at 4.5-5.5 m and never over 6 m.

Applicable Codes

  • DB37/T 5060-2016 海绵城市设计规程 第5.2.7条
  • DB11/T 685-2021 海绵城市雨水控制与利用工程设计规范 第7.2.12条
  • DB3201/T 1150-2023 透水铺装建设与运行维护技术规范 第5.3.1条
  • DB 6501/T 039-2022 乌鲁木齐市海绵城市建设透水铺装技术指南 第3.1、3.2节
  • CJJ/T 188-2012 透水砖路面技术规程
  • CJJ/T 190 透水沥青路面技术规程
  • CJJ/T 135 透水水泥混凝土路面技术规程
  • CJJ 1 城镇道路工程施工与质量验收规范
  • JGJ 63 混凝土用水标准

Scope of the question

The structural layering of sponge-city permeable paving (permeable brick paving) and the materials, thicknesses, porosities, compaction and key control indices of the surface, levelling, permeable base, permeable subbase (cushion) and subgrade. The layering is both a design requirement and the build-up basis for splitting quota items layer by layer.

Core conclusions

1. Structural layers (terms) A permeable brick pavement is a pavement structure system of certain thickness, void ratio and layered structure with permeable bricks as the surface, comprising the permeable brick surface, levelling layer, base and cushion (DB 6501/T 039-2022 Section 3.1, from CJJ/T 188-2012 Article 2.1.1, modified). Practice says: surface - levelling layer - permeable base - permeable subbase (cushion) - subgrade.

2. Layer requirements (DB37/T 5060-2016 Sponge City Design Code, Article 5.2.7)

  • Surface thickness preferably 60-80 mm, of pervious concrete, permeable bricks or turf bricks; levelling layer 20-40 mm; cushion 100-300 mm, of no-fines concrete, gravel, sand, sand-gravel or combinations.
  • Surface porosity at least 20%; permeable cushion at least 30%.
  • The structure shall meet bearing and frost requirements.
  • Semi-permeable structures may be used where subgrade strength and stability risks are high.
  • Where soil permeability is limited, drains or drainage boards go in the permeable base.
  • Over basement roofs, the cover soil shall be at least 600 mm with a drainage layer.

3. Levelling, base and subbase materials and seepage pipes (DB11 685-2021 Article 7.2.12)

  • The levelling layer's permeability coefficient shall be not less than the surface's, preferably medium-coarse sand or fine-stone pervious concrete;
  • The permeable base may be graded crushed stone, porous cement-stabilised crushed stone or pervious concrete;
  • Base thickness per the ground load intensity;
  • The permeable subbase may be graded crushed stone, graded gravel, natural graded sand-gravel, crushed-gravel blends or macadam;
  • In high-water-table, severe-cold and over-basement cases, seepage pipes go in the subbase, of materials meeting load and frost-heave requirements.
  • Build-up choices: semi-permeable and light-load fully permeable structures have no permeable base; semi-permeable structures have no permeable subbase; large permeable plazas and important roads also need seepage pipes in the subbase.
  • Surface and cushion need enough voids to detain rain; omitting or mis-setting the permeable cushion impairs infiltration.

4. Construction and material control (DB3201/T 1150-2023 Technical Code for Permeable Pavement Construction and O&M, Article 5.3.1)

  • The permeable brick surface follows CJJ/T 188.
  • Levelling layer: dry-hard cement mortar, crushed stone or stone chips, or dry sand. Mortar cement-sand preferably 1:3; chips with elongated-flaky content under 10%, fines under 1%, clay lumps under 0.5%, moisture under 2%; sand fines under 2%, clay lumps under 1%, moisture under 3%. Sand layers spread by screed, thickness not under 20 mm, dense and firmly bonded to the bricks.
  • Permeable base: strong, permeable, water-stable materials, preferably graded crushed stone or pervious cement concrete (graded stone per CJJ 1). Pervious concrete aggregate single-graded 5-10 mm, maximum 15 mm; P.O 42.5+ Portland or ordinary Portland cement; water per JGJ 63; chlorine-free admixtures preferred. Reference mix: water-cement about 0.38, cement 245-270 kg/m3, stone about 1600 kg/m3. Wet and compact with plate vibrators before casting, avoiding over-vibration; provide temperature and construction joints at 4.5-5.5 m, never over 6 m, or per design; cure moist promptly, avoiding wet-dry cycling.
  • Permeable subbase: preferably permeable sand or graded crushed stone. Medium-coarse sand or natural graded sand-gravel: fines not over 5%, clay lumps under 2%, moisture under 3%; graded crushed stone of tough, wear-resistant crushed granite or limestone, flat and elongated particles not over 10%, free of clay lumps and vegetation. Water lightly and compact on spreading, compaction at least 93%.
  • Subgrade: soil, depth and compaction per design, survey results checked before construction; roll from edges to centre to the design compaction; where rollers do not suit, compact manually or with vibrating rammers.

5. Pricing relation Permeable paving is not one single build-up: surfaces (permeable bricks, pervious concrete, pervious asphalt, turf bricks, pebbles / gravel), bases (graded stone, porous cement-stabilised stone, pervious concrete) and cushions (sand, sand-gravel, graded stone, no-fines concrete) all differ, as do work contents (mixing, spreading, compaction, jointing, curing) - so both design and pricing fix the build-up layer by layer, listing layer by layer, never as one blanket permeable paving item.

Applicability limits

  • Thicknesses and porosities are mostly preferable values: 60-80 / 20-40 / 100-300 mm from Shandong DB37/T 5060-2016 5.2.7; Nanjing DB3201/T 1150-2023 says only not under 20 mm for the levelling layer; Beijing DB11 685-2021 stresses permeability not below the surface and base thickness by load. Follow the project's local standard - no cross-region values.
  • Scope is fully / semi-permeable permeable-brick paving; sealed (impermeable) paving excluded. Semi-permeable structures suit high subgrade risk cases and lack the permeable base or subbase (per build-up) - do not list nonexistent layers.
  • Over basement roofs and in severe-cold or high-water-table areas, the extras (600 mm cover, drainage layer, seepage pipes) price and build separately.
  • Dedicated structures follow CJJ/T 188 (bricks), CJJ/T 190 (asphalt) and CJJ/T 135 (pervious concrete); this card replaces neither them nor the local quota items' descriptions.

Further reading

  • DB37/T 5060-2016 Article 5.2.7; DB11 685-2021 Article 7.2.12; DB3201/T 1150-2023 Article 5.3.1 (5.3.1.1-5.3.1.5); DB 6501/T 039-2022 Sections 3.1-3.2; CJJ/T 188-2012, CJJ/T 190, CJJ/T 135, CJJ 1, JGJ 63.

Keywords

  • 透水铺装
  • 透水砖铺装
  • 透水砖路面结构分层
  • 透水基层
  • 透水垫层
  • 找平层
  • 孔隙率
  • 海绵城市透水铺装